MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Armacell ArmaSound® RD240 Sound Adsorption Insulation
Categories: Other Engineering Material

Material Notes: Description: Highly-flexible, hydrophobic, open-cell acoustic insulation material with complex pore geometry.

Special features: Excellent sound adsorption performance

Application: In general applications ArmaSound® RD240 is used as acoustic insulation material with excellent sound adsorption performance in a variety of different applications e.g. fan-coil units, duct linings, cabinet linings, chiller systems, enclosures, pipelines. In industrial applications ArmaSound® RD240 is used as an important component of Arma-Sound Industrial systems to provide acoustic insulation on industrial pipework and vessels ensuring reduction of sound transmission. Further industrial application area is sound adsorption performance of enclosures.

Information provided by Armacell®

Vendors:
Available Properties
  • Density, ASTM D1622
  • Water Absorption, AGI Q 136
  • Absorption Coefficient, NRC, Sound
  • Absorption Coefficient, NRC, Sound
  • Absorption Coefficient, NRC, Sound
  • Absorption Coefficient, NRC, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Absorption Coefficient, Sound
  • Tensile Strength, ISO 1798, MD
  • Elongation at Break, ISO 1798, MD
  • Tear Strength, ISO 34-1, MD/CD
  • Thermal Conductivity, EN 12667
  • Maximum Service Temperature, Air, EN 14706 EN 14304
  • Minimum Service Temperature, Air, EN 14706 and EN 14304
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.