MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Bostik 915FS™ Polyurethane Sealant
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Bostik 915FS™ is a one-component, smooth fast setting polyurethane sealant/adhesive capable of dynamic joint movement totaling 70% of original joint geometry (±35%). The sealant cures to a tough, flexible rubber when exposed to moisture present in the atmosphere. Bostik 915FS™ has a consistency like toothpaste, its physical properties will remain relatively stable over time and in varying weather conditions. Its physical properties are relatively unchanged over a wide temperature range, -40°F to 150°F (-40°C to 66°C). Where textured appearance is needed, please use Bostik 916™ or Bostik 2000 Textured™.

Key Features:

  • Fast skin time enables quicker top coat
  • Bonds to Kynar coated metals
  • Best in class warranty
Basic Uses: Bostik 915FS™ is designed for sealing expansion and control joints, for use under deck coatings, for sealing various roofing and siding applications, such as metal roofs, gutters, roof tile applications, and for sealing perimeters of doors, windows, and other wall penetrations. Bostik 915FS™ cures to form a durable, flexible bond with most building materials in any combination including stone, masonry, ceramic, wood, steel, aluminum, bondarized, and Kynar coated metals, and many other synthetic materials.

Mechanical property data reported after 14 days cure at 77°F and 50% RH.

Information provided by Bostik

Vendors:
Available Properties
  • Hardness, Shore A, ASTM C661
  • Tensile Strength at Break, ASTM D412
  • Elongation at Break, ASTM D412
  • 100% Modulus, ASTM D412
  • Peel Strength, ASTM C794
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, Skin Time
  • Cure Time, Full
  • Working Life, Tool/Work Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.