Notes: Monprene RG-18200 series is a group of unfilled high performance thermoplastic elastomer with high flow specifically designed for EU injection molded regulated applications including food contact, toys, and children’s products. Monprene RG-18260 is a low density, medium hardness grade that complies with various US FDA regulations and EU directives for food contact and toy safety and is suitable for injection molding. Availability: Asia Pacific; Europe; Latin America; North America Features: Food Contact Acceptable; Good Adhesion; Good Colorability; Good Processability; Low Density; Low Specific Gravity; Lubricated; Medium Hardness; Without Fillers Uses: Closures; Consumer Applications; Cosmetic Packaging; Food Containers; Food Packaging; Food Service Applications; Gaskets; Handles; Kitchenware; Lids; Non-specific Food Applications; Rubber Replacement; Toothbrush Handles; Toys RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding Preliminary data. Information provided by Teknor Apex |