MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Dow Dow™ DFDA-7059 NT7 LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Product Description: Dow DFDA-7059 NT7 linear low density polyethylene is an ethylene-butene copolymer which is supplied in pellet form. It is generally recommended for slot cast thin film applications requiring both clarity and toughness. It is excellent in coextruded, slot cast stretch wrap. This resin is also suitable for use in hose and tube applications.
Main Characteristics:
  • High clarity
  • High tensile strength
  • High elongation
  • Good puncture resistance
Complies with: US FDA 21 CFR 177.1520©3.2a; Canadian HPFB No Objection; EU No 10/2011. Consult the regulations for complete details.

Availability: Europe; Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520©3.2a; Canadian HPFB No Objection; EU No 10/2011

Form: Pellets

Processing Method: Blown Film; Cast Film

Information provided by The Dow Chemical Company

Vendors:
Available Properties
  • Density, ASTM D792
  • Melt Flow, ASTM D1238
  • Tensile Strength at Break, ASTM D638, Plaque molded and tested in accordance with ASTM D4976
  • Tensile Strength, Yield, ASTM D638, Plaque molded and tested in accordance with ASTM D4976
  • Film Elongation at Break, MD, ASTM D882, Cast Film
  • Film Elongation at Break, TD, ASTM D882, Cast Film
  • Elongation at Break, ASTM D638, Plaque molded and tested in accordance with ASTM D4976
  • Elongation at Yield, ASTM D638, Plaque molded and tested in accordance with ASTM D4976
  • Flexural Modulus, ASTM D790B, 2% Secant, Plaque molded and tested in accordance with ASTM D4976
  • Elmendorf Tear Strength MD, ASTM D1922, Cast Film
  • Elmendorf Tear Strength TD, ASTM D1922, Cast Film
  • Dart Drop Test, ASTM D1709A, Cast Film
  • Film Tensile Strength at Break, MD, ASTM D882, Cast Film
  • Film Tensile Strength at Break, TD, ASTM D882, Cast Film
  • Melting Point
  • Haze, ASTM D1003, Cast Film
  • Gloss, ASTM D2457, 45°, Cast Film
  • Melt Temperature, Extrusion
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Dow Chemical

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.