MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Master Bond Super Gel 9 Two component urethane modified epoxy gel-like system
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Cures to a low Shore A hardness
  • Excellent optical clarity
  • Easy to remove
  • Ideal for retrievability
  • Convenient handling
  • Room temperature curing
Product Description: Master Bond Super Gel 9 is a two component, urethane modified epoxy system that cures readily at room temperature to form a soft, resilient, gel-like system with good dimensional stability. Its hardness is exceptionally low, about 5-10 Shore A. One can accomplish retrievability with a sharp knife or razor blade and Super Gel 9 will not shatter. It has a very convenient two to one mix ratio by weight or volume, along with an extremely low viscosity and exotherm enabling it to be cast in larger sections up to 2-3 inches thick. Super Gel 9 has wonderful optical clarity. The combination of its easy handling and cured properties enables this versatile system to be used in a variety of applications, especially the encapsulation of sensitive electronic parts and sealing delicate optical components. It can also be used in acoustical applications where dampening properties may be desirable. This exceptional softness allows it to be easily repairable and confers it with unsurpassed thermal cycling and mechanical shock resistance. Super Gel 9 bonds well to an array of substrates, such as metals, glass, ceramics and many rubbers and plastics. It has a remarkably long working life of 7-9 hours depending on the mass that is mixed (the smaller the mass, the longer the working life). It has very good chemical resistance to water, oils and fuels. The service temperature range is -100°F to +200°F. The color of both Parts A and B are clear. This multi-functional system is widely used in the aerospace, electronic, optical, electro-optical and other specialty industries where this unique blend of properties is needed.

Product Advantages:

  • Easy handling; two to one mix ratio by weight or volume; low viscosity
  • Very low exotherm; remarkably long working life
  • Exceptionally soft and resilient
  • Good dimensional stability
  • Easily repairable; widely used for retrieving components
  • Often used in conjunction with sensitive electronic and optical components

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, Mixed
  • Viscosity, Part A
  • Hardness, Shore A
  • Tensile Strength
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Refractive Index
  • Cure Time, 24-48 hours at 75°F, plus 140-150°F
  • Cure Time
  • Working Life, After mixing, 200 gram batch
  • Working Life, After mixing, 100 gram batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.