MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
PoolKemie EPOCOL 890 + EH 890 Epoxy adhesive
Categories: Polymer; Thermoset; Epoxy

Material Notes: Introduction: Two components modified, unfilled and thixotropic epoxy system. Easy mixing ratio 2:1 by volume. Solvent free. Sag resistance till 5 mm. High toughness. Good thermal resistance. It is advisable to use the system at a temperature not lower than 20-25°C.

Application: Structural thermal resistant bonding. Adhesive for assembly of composite materials, metals, automotive components, sport components.

Cured: 24 h at R.T. (23±2° C) + 15 h at 60° C

Information provided by Poolkemie

Vendors:
Available Properties
  • Specific Gravity, ASTM D 1475, Hardener
  • Specific Gravity, ASTM D 792, Cured
  • Specific Gravity, ASTM D 1475, Resin
  • Viscosity, Initial mixture, EN13702-2
  • Hardness, Shore D, ASTM D 2240, Cured
  • Tensile Strength, ASTM D 638, Cured
  • Elongation at Break, ASTM D 638, Cured
  • Flexural Strength, ASTM D790, Cured
  • Flexural Modulus, ASTM D790, elastic, cured
  • Shear Strength, ASTM D 1002, by tension, Inox steel AISI 316 cured 6h RT
  • Shear Strength, ASTM D 1002, by tension, Inox steel AISI 316 cured 24h RT
  • Shear Strength, ASTM D 1002, by tension, Aluminum cured 2h 80°C
  • Shear Strength, ASTM D 1002, by tension, Carbon composite cured 24h RT
  • Shear Strength, ASTM D 1002, by tension, Inox steel AISI 316 cured 7days RT
  • Shear Strength, ASTM D 1002, by tension, Inox steel AISI 316 cured 2h 80°C
  • Shear Strength, ASTM D 1002, by tension, Aluminum cured 2h 80°C
  • Shear Strength, ASTM D 1002, by tension, Carbon composite cured 2h 80°C
  • Maximum Service Temperature, Air
  • Glass Transition Temp, Tg, ASTM D 3418, Cured
  • Glass Transition Temp, Tg, ASTM D 3418, Cured
  • Glass Transition Temp, Tg, ASTM D 3418, Cured
  • Cure Time, Setting time
  • Pot Life, 100 ml, 40 mm
  • Gel Time, 15 ml, 5 mm
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.