MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
ChevronTexaco Polystar® RB NLGI Grade 2
Categories: Fluid; Lubricant; Urea Gellant

Material Notes: Texaco Polystar RB 2 delivers value through:
  • Ability to meet bearing OEM requirements — Suitable for high rpm operations, operating temperatures ranging from -34°C to 204°C (-30°F to 400°F) and offers excellent rust protection in the presence of both salt and fresh water.
  • Excellent oxidation stability — Provides excellent bearing life with continuous service possible at temperatures up to 160°C (320°F). For short exposure, the maximum is 200°C (392°F).
  • Corrosion protection — Provides superior water resistance and protection of bearings against rust and corrosion.
  • Good low shear stability — Will not soften excessively under prolonged low shear stress.

Texaco Polystar RB 2 is a high temperature ball and roller bearing grease.

It is formulated with high quality base stocks, a synthetic polyurea ashless organic thickener, and high performance rust and oxidation inhibitors (the latter to provide superior rust protection in severe applications).

Texaco Polystar RB 2 is specifically designed to meet the factory-fill performance requirements of the major manufacturers of rolling element bearings.

Texaco Polystar RB 2 is recommended:

  • For use in antifriction bearings operating at high speeds (speeds up to 500,000 DN).
  • Where the operating temperatures are on the order of 150°C (302°F) and higher.
  • Where there is a likelihood that water or salt water will get into the bearings.

It performs satisfactorily in bearings at temperatures as low as -34°C (-30°F).

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.
  2. Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.
  3. Determined on mineral oil extracted by vacuum filtration.

CPS Number: 221915; MSDS Number: 8998

Vendors:
Available Properties
  • Viscosity Measurement, Viscosity Index, See Note 3.
  • Saybolt Viscosity at 100°F, See Note 3.
  • Saybolt Viscosity at 210°F, See Note 3.
  • Kinematic Viscosity at 40°C (104°F), See Note 3.
  • Kinematic Viscosity at 100°C (212°F), See Note 3.
  • Penetration P(60), 1/10 mm, Unknown Amount of Work, 25°C (77°F)
  • Maximum Service Temperature, Air, See Note 2.
  • Minimum Service Temperature, Air, See Note 1.
  • Flash Point
  • Dropping Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.