MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Go Yen Chemical DPHP
Categories: Other Engineering Material

Material Notes: Di(2-Propyl Heptyl) phthalate (DPHP) is a phthalate ester plasticiser based on isomeric C10 alcohols. DPHP is a nearly colourless, clear and practically anhydrous liquid with a hardly noticeable odour. It is soluble in the usual organic solvents and is miscible and compatible with all of the monomeric plasticisers commonly used in PVC. DPHP is almost insoluble in water. Owing to its low volatility, DPHP is quite suitable for higher temperature applications such as wire & cable and automotive interior trim. With excellent weather resistance, it makes DPHP a good choice for outdoor applications such as roofing membranes and tarpaulins. DPHP can be used to substitute DINP, of which the weather resistance is better and the cost is lower.

Advantages:

  • Excellent weather resistance
  • Good anti-fogging properties
  • Wonderful thermal aging properties
  • Smell lighter
  • Higher output of thermoplastic processing
  • With good compatibility with PVC
Usage:
  • Wires & Cables
  • Automotive
  • Leather
  • Roofing membranes
  • Tarpaulines
  • Outdoor PVC products

Information provided by Go Yen Chemical

Vendors:
Available Properties
  • Density, ASTM D4052
  • Acid Value, ASTM D1045, [mg-KOH/g]
  • Moisture Content, ASTM E203
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.