Characteristics: Low melt flow rate Impact Block Copolymer polypropylene; very high impact/stiffness balance. Recommended for: Compounding for the automotive industry; sheet extrusion, Cartonplast; high volume extrusion blow molding containers; extrusion thermoforming of containers that require conservation at temperatures below 0 ºC; extrusion and injection molding general purpose applications. Information provided by Esenttia by Propilco |