MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Chesterton 772 Premium Nickel Anti-Seize Compound
Categories: Fluid; Lubricant

Material Notes: Description: Chesterton® 772 Premium Nickel Anti-Seize Compound is formulated with ultra pure raw materials. This permits 772 Premium Nickel Anti-Seize Compound to conform to most applicable equipment specifications which restrict the levels of halogens, sulfur and low melting point metals. Chesterton 772 Premium Nickel Anti-Seize Compound is an assembly lubricant combining the extreme pressure, corrosion resistant anti-seize abilities of colloidal nickel and graphite in an oil suspension which will withstand temperatures up to 1425°C (2600°F). The product seals and protects metal parts under extreme conditions by providing an ultra-thin coating of particles. The particles form an anti-friction barrier that will not burn, wash or scrape off. The barrier formed prevents pitting from the galvanic action between dissimilar metals that could occur if the metals were not separated. Because nickel is a hard metal, it will withstand severe pressures without flattening or hardening. The microscopic asperities on metal parts do not come in contact as the ultra-fine nickel particles fill surface irregularities and keep them separated. Chesterton 772 Premium Nickel Anti-Seize Compound has a balanced coefficient of friction, threads are not stretched and more accurate load values are possible during assembly. The product saves threads and parts for reuse by preventing galling damage and breakage during opening. 772 Premium Nickel Anti-Seize Compound will not wash off in either fresh or salt water. It can be used indoors, outdoors and in marine applications. The product meets MIL-A-907F

Features:

  • Ultra-Fine Particle Size
  • Withstands Extreme Pressure
  • Corrosion Resistant
  • Meets MIL A-907F
  • Certified lot analysis
  • Effective at 1425°C(2600°F)
  • Applicable where use of copper is prohibited
  • Water Resistant
  • GE TIL 1137-3R1
  • GE D50YP12
  • GE NEDC-31735P

Applications: Eases mechanical assembly of bolts, studs, flanges, press fits, pump sleeves, valve stems, screws, bushings, gaskets, bearings, etc. Eases disassembly by preventing seizure and inhibiting rust and corrosion up to 1425°C (2600°F). Saves threads and parts for reuse by preventing galling damage and breakage during opening. Use on steel and stainless steel, iron, aluminum, copper, brass, titanium etc. in the automotive and chemical industries, in foundries, utilities, and refineries. Should not be used on oxygen systems.

Information provided by Chesterton

Vendors:
Available Properties
  • Specific Gravity
  • Particle Size
  • Four Ball Extreme Pressure, Load Wear Index, ASTM D2596, DIN 51 350, 101,505 psi
  • Four Ball Extreme Pressure, Weld Load, ASTM D2596, DIN 51 350
  • Penetration, ASTM D217, ISO2137
  • K Factor (Wear Factor), Skidmore - Wilhelm Method
  • Maximum Service Temperature, Air
  • Dropping Point, ASTM D566, ISO2176
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.