MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Schmolz + Bickenbach UGIMA 303 UX® Stainless Steel Bar
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Description: 303 UGIMA UX® is an improved machining grade produced only by Ugitech, providing the ultimate level of machinability available in an austenitic stainless steel. 303 UGIMA UX® features the added benefit of increased cold formability when compared with that of standard type 303 stainless steels. The combination of machinability and cold formability affored by 303 UGIMA UX® is great, and provides the optimum solution for even the most difficult fabrication challenges. Other advantages offered by 303 UGIMA UX® when compared with standard type 303 stainless steels include increased corrosion resistance in certain media, and ability to withstand moderate amounts of cold deformation with no significant increase in magnetic permeability. 303 UGIMA UX® builds upon the proprietary UGIMA® technology with the addition of copper, allowing for good machinablity across a wide range of operations and cutting conditions. It allows for machinability at both low and high speeds, in cam-driven and CNC machines, and with high-speed Steel or carbide tooling. Machine shops using 303 UGIMA UX® have experienced consistent success regardless of machine, operation, tooling, or cutting conditions. From lot to lot, 303 Ugima UX® is engineered to give the same high performance every time without surprises.

Information provided by Schmolz + Bickenbach

Key Words: EN 10088-3 1.4570; X6CrNiCuS18-9-2
Vendors:
Available Properties
  • Density
  • Hardness, Brinell, Turned Bars
  • Hardness, Brinell, Cold Drawn Bars
  • Tensile Strength, Turned Bars
  • Tensile Strength, Cold Drawn Bars
  • Tensile Strength, Heat Treatment
  • Tensile Strength, Yield, Turned Bars
  • Tensile Strength, Yield, Cold Drawn Bars
  • Tensile Strength, Yield, Heat Treatment
  • Elongation at Yield, Cold Drawn Bars
  • Elongation at Yield, Turned Bars
  • Elongation at Yield, Heat Treatment
  • Reduction of Area, Cold Drawn Bars
  • Reduction of Area, Turned Bars
  • Modulus of Elasticity
  • Electrical Resistivity
  • CTE, linear
  • Thermal Conductivity
  • Hot-Working Temperature, Forging range
  • Hot-Working Temperature, Heat in range
  • Carbon, C
  • Chromium, Cr
  • Copper, Cu
  • Iron, Fe
  • Manganese, Mn
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Schmolz + Bickenbach (Swiss Steel International)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.