MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Lord Adhesives 7555 Urethane Adhesive/Sealant, 7555-A/C Adhesive System
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: LORD® 7555 adhesive/sealant is an equal-mix, two-component bright white urethane adhesive/sealant system used to bond and seal a variety of plastics and prepared metals. After opening, protect adhesive/sealant from excessive exposure to moisture by replacing protective cap on the cartridge.

Features: full-bodied urethane formula holds bead pattern on horizontal surfaces, allowing for greater processing flexibility; non-slumping. LORD 7555-A/7555-C adhesive/sealant develops handling strength within 60 minutes, ideal for smaller bonding and sealing applications. offers immediate paint time, improving throughput. LORD 7555-A/7555-E adhesive/sealant offers longer working time, allowing for use on larger projects where more time is required. does not require explosion-proof equipment. no VOC content; does not contain ozone depleting chemicals. resists sunlight, weathering, humidity and salt spray; bright white color will not yellow. solvent resistant when cured. Painting and most cleaning processes do not affect bond strength.

All information provided by Lord.

Vendors:
Available Properties
  • Density, A Resin
  • Density, C Curative
  • Solids Content, by weight, mixed with resin
  • Volatile Organic Compounds (VOC) Content
  • Viscosity Measure, A Resin
  • Viscosity Measure, C Curative
  • Elongation at Break, Cured, mixed with resin
  • Flash Point, closed cup, A Resin
  • Flash Point, closed cup, C Curative
  • Pot Life, time to handling strength, mixed with resin
  • Working Life, working time, mixed with resin
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.