MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
BYK Advitrol® 50 Castor-based thixotropes
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Advitrol 50 are castor-based thixotropes suitable for a wide range of solvent systems. Compared to organoclays, castor-based thixotropes are significantly more thixotropic. This means that paints and coatings formulated with castor-based thixotropes exhibit shearthinning that does not immediately rebuild upon removal of the shear forces. This type of rheology presents several advantages, mainly in application properties. It is often said that these coatings exhibit a “buttery” feel during brushing. These thixotropes also provide a good balance between sag and leveling and usually are more effective in pigment suspension when compared to organoclay gellants.

Applications: Advitrol 100 & Advitrol 50 may be used in trade sales paints, industrial maintenance coatings, marine coatings, and product finishes. Advitrol 100 is especially useful in formulating high build epoxies and vinyls. Aliphatic, aromatic, and oxygenated solvents are all suitable for the Advitrol types. Note that as the KB Value of the solvent system increases, the incorporation temperature range narrows and the minimum and maximum incorporation temperatures decrease.

Information provided by Southern Clay Products

Vendors:
Available Properties
  • Density
  • Particle Size, 100%
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
former Southern Clay Products

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.