Available Properties |
---|
- Density, Cured Unfilled Resin
- Viscosity, Neat Resin
- Storage Temperature
- Tensile Strength, 90° orientation, Actual 47.3% VF
- Tensile Strength, 0° orientation, Actual 47.3% VF
- Tensile Strength, 90° orientation, Normalized 55% VF
- Tensile Strength, 0° orientation, Normalized 55% VF
- Tensile Strength, 90° orientation, Actual 47.3% VF
- Tensile Strength, 0° orientation, Actual 47.3% VF
- Tensile Strength, 90° orientation, Normalized 55% VF
- Tensile Strength, 0° orientation, Normalized 55% VF
- Tensile Modulus, 90° orientation, Actual 47.3% VF
- Tensile Modulus, 0° orientation, Actual 47.3% VF
- Tensile Modulus, 90° orientation, Actual 47.3% VF
- Tensile Modulus, 0° orientation, Actual 47.3% VF
- Tensile Modulus, 90° orientation, Normalized 55% VF
- Tensile Modulus, 0° orientation, Normalized 55% VF
- Tensile Modulus, 90° orientation, Normalized 55% VF
- Tensile Modulus, 0° orientation, Normalized 55% VF
- Flexural Strength, 90° orientation, Actual 47.3% VF
- Flexural Strength, 0° orientation, Actual 47.3% VF
- Flexural Strength, 90° orientation, Actual 47.3% VF
- Flexural Strength, 0° orientation, Actual 47.3% VF
- Flexural Strength, 90° orientation, Normalized 55% VF
- Flexural Strength, 0° orientation, Normalized 55% VF
- Flexural Strength, 90° orientation, Normalized 55% VF
- Flexural Strength, 0° orientation, Normalized 55% VF
- Flexural Modulus, 0° orientation, Actual 47.3% VF
- Flexural Modulus, 90° orientation, Actual 47.3% VF
- Flexural Modulus, 90° orientation, Actual 47.3% VF
- Flexural Modulus, 0° orientation, Actual 47.3% VF
- Flexural Modulus, 0° orientation, Normalized 55% VF
- Flexural Modulus, 90° orientation, Normalized 55% VF
- Flexural Modulus, 90° orientation, Normalized 55% VF
- Flexural Modulus, 0° orientation, Normalized 55% VF
- Compressive Strength, 90° orientation, Actual 47.3% VF
- Compressive Strength, 0° orientation, Actual 47.3% VF
- Compressive Strength, 90° orientation, Actual 47.3% VF
- Compressive Strength, 0° orientation, Actual 47.3% VF
- Compressive Strength, 90° orientation, Normalized 55% VF
- Compressive Strength, 0° orientation, Normalized 55% VF
- Compressive Strength, 90° orientation, Normalized 55% VF
- Compressive Strength, 0° orientation, Normalized 55% VF
- Compressive Modulus, 90° orientation, Actual 47.3% VF
- Compressive Modulus, 0° orientation, Actual 47.3% VF
- Compressive Modulus, 90° orientation, Actual 47.3% VF
- Compressive Modulus, 0° orientation, Actual 47.3% VF
- Compressive Modulus, 90° orientation, Normalized 55% VF
- Compressive Modulus, 0° orientation, Normalized 55% VF
- Compressive Modulus, 90° orientation, Normalized 55% VF
- Compressive Modulus, 0° orientation, Normalized 55% VF
- Bearing Yield Strength, Actual 47.3% VF
- Poissons Ratio, 0° orientation, Actual 47.3% VF
- Poissons Ratio, 90° orientation, Actual 47.3% VF
- Poissons Ratio, ±45°, Actual 47.3% VF
- Shear Strength, Interlaminar, Actual 47.3% VF
- Shear Strength, Interlaminar, Actual 47.3% VF
- Shear Strength, In Plane, Actual 47.3% VF
- Maximum Service Temperature, Air
- Glass Transition Temp, Tg, following 180°C (356°F) cure
- Gel Time
- Shelf Life
|
| | |