MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
IBC Advanced Alloys Thermal Mould™ Super Mold and Die Copper Alloy, Beryllium-Free
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Thermal Mould™ Super is manufactured to provide a combination of high strength and hardness properties coupled with superior thermal properties. This range of properties makes Thermal-Mould™ Super the premier material for copper alloy molds and a wide range of other applications from oil and gas to aerospace.

Information provided by IBC Advanced Alloys.

Vendors:
Available Properties
  • Density
  • Hardness, Rockwell C, Heat Treated plate and round bars
  • Tensile Strength, Heat Treated plate and round bars
  • Tensile Strength, Yield, Heat Treated plate and round bars
  • Elongation at Break, Heat Treated plate and round bars
  • Modulus of Elasticity
  • CTE, linear
  • Thermal Conductivity
  • Melting Point
  • Chromium, Cr
  • Copper, Cu, As Balance
  • Nickel, Ni
  • Silicon, Si
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.