MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Aptek UVISTAKE 7205LM-PMF UV Curing, Low Outgassing, Urethane staking compound
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: UVISTAKE 7205LM-PMF is a 100% solids, thixotropic, one component, premixed frozen, electrically insulating, urethane system designed for the attachment and staking of electrical/electronic components mounted on printed circuit boards. This system provides an excellent combination of flexibility and strength for demanding applications where toughness is required for the management of thermomechanical stresses. UVISTAKE 7205LM-PMF will become tack free when exposed to the proper UV light radiation. The staking compound will fully post cure in exposed and shaded areas in 14 days at 25ºC and 50% relative humidity, as an alternative, the post cure for the staking compound in both exposed and shaded areas may be accelerated with low to moderate heat.

Multicure mechanism for complete cure in shaded areas underneath components; Good flexibility for reduced stress in the encapsulation of sensitive glass-bodied components; Meets NASA condensable volatile requirements for high vacuum environments; Highly reversion resistant for good physical stability under high heat and humidity environments; Excellent adhesion to plastic/metal components and substrates; More rigid version (95A) available as UVISTAKE 7205-PMF; Packaged in syringes for convenient dispensing; No TDI, no toxic solvents, no free acrylic acid for safety

Information provided by Aptek Laboratories, Inc.

Vendors:
Available Properties
  • Density, ASTM D1475
  • Outgassing - Total Mass Loss, Cured property; at 10E-6 torr; ASTM E595
  • Collected Volatile Condensable Material, Cured property; at 10E-6 torr; ASTM E595
  • Hardness, Shore A, Cured property; ASTM D2240
  • Volume Resistivity, Cured property; ASTM D257
  • Dielectric Constant, ASTM D150, Cured property
  • Dielectric Strength, ASTM D149, Cured
  • CTE, linear, ASTM E831-86, Cured property; alpha 2
  • Glass Transition Temp, Tg, Cured property; ASTM E831-86
  • Flash Point, ASTM D92
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.