MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
ExxonMobil Exact ™ 9182 Ethylene Alpha Olefin Copolymer
Categories: Polymer; Thermoplastic

Material Notes: Plastomers are ethylene alpha olefin copolymers that bridge the gap between elastomers and plastics. With rubber-like properties and the processability of plastic, they are used as polymer modifiers to provide unique properties in flexible packaging, molded and extruded products, and foamed compounds.  Benefits:  Flexible packaging – enhanced toughness, clarity and sealing performance, Molded and extruded products – improved impact strength and flexibility, Foamed compounds – added durability to lightweight shoe mid soles  With characteristics that improve strength and flexibility, Exact plastomer resins’ rubber-like properties support product durability and processability.  Exact 9182 is an ethylene butene copolymer produced using ExxonMobil's proprietary metallocene catalyst technology.  This resin is compatible with polyolefins like polypropylene, polyethylene, and ethylene-vinyl acetate copolymer resin. 

Availability:  Asia Pacific (* product may not be available in one or more countries in the identified availability regions.  Contact your sales rep for complete country availability.)

Information provided by ExxonMobil.

Vendors:
Available Properties
  • Density, ExxonMobil Method
  • Melt Flow, ExxonMobil Method
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength at Break, ASTM D412
  • Elongation at Break, ASTM D412
  • 100% Modulus, ASTM D412
  • Flexural Modulus, 1% Secant, ASTM D790
  • Melting Point, ExxonMobil Method, Peak
  • Crystallization Temperature, ExxonMobil Method
  • Vicat Softening Point, ExxonMobil Method
  • Glass Transition Temp, Tg, ExxonMobil Method
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Exxon Chemical

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.