MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Sandvik Sanicro 53 Welding wire
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Sanicro 53 is a nickel-chrome-cobalt-molybdenum alloy of type alloy 617. It has an excellent resistance to high temperature corrosion such as oxidation and carburization. The weld metal provides a combination of excellent metallurgical stability and strength in short and long term exposure to temperatures up to 1100°C (2012°F). Applications for Sanicro 53 are found in high temperature heat exchangers and valves, furnace tubing in the petrochemical industry, radiant heat tubes, gas turbines, components subjected to high temperatures in the chemical processing industry and components for power plants. Sanicro 53 is suitable for joining heat resistant nickel alloys, heat resistant austenitic and cast alloys such as:
  • UNS N08810 (1.4958)
  • UNS N08811 (1.4959)
  • UNS N06617 (2.4663)
Sanicro 53 can also be used for surfacing.

Information provided by Sandvik

Vendors:
Available Properties
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Charpy Impact
  • Charpy Impact
  • Aluminum, Al, Filler metal
  • Carbon, C, All-weld metal
  • Carbon, C, Filler metal
  • Chromium, Cr, Filler metal
  • Chromium, Cr, All-weld metal
  • Cobalt, Co, All-weld metal
  • Cobalt, Co, Filler metal
  • Iron, Fe, All-weld metal
  • Iron, Fe, Filler metal
  • Manganese, Mn, All-weld metal
  • Manganese, Mn, Filler metal
  • Molybdenum, Mo, Filler metal
  • Molybdenum, Mo, All-weld metal
  • Nickel, Ni, Filler metal
  • Nickel, Ni, All-weld metal
  • Phosphorus, P, Filler metal
  • Silicon, Si, All-weld metal
  • Silicon, Si, Filler metal
  • Sulfur, S, Filler metal
  • Titanium, Ti, Filler metal
  • Tungsten, W, All-weld metal
  • Tungsten, W, Filler metal
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.