MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Go Yen Chemical GYC-AT-300B Highly Effective Anti-Static Agent for Multiple Plastics
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Intro: GYC-AT-300B is an anti-static agent comes in pellet form that is developed by GO YEN CHEMICAL INDUSTRIAL CO., LTD. (GYC GROUP). The design caters mainly to the products that a pellet compounding is required such as plastic pellet, elastomer, etc. The anti-static ingredient is 100% concentrated in GYC-AT-300B through the unique thermocompression technique which makes GYCAT-300B effectively reduce the surface resistance value and provide extraordinary anti-static performance to plastics, rubbers, elastomers, and so forth. GYC-AT-300B feature outstanding compatibility and processing behavior during the pellet compounding while the traditional anti-static agents in liquid or powder form offers weak processing behavior. Compared to the traditional anti-static plastic compound, GYC-AT-300B are concentrated pellets with no plastic material contained and can be used in any plastics and elastomers. GYC-AT-300B is ease of operating and produces no dust that can be directly added or used for the applications of extrusion molding, injection molding, and blown film molding.

Features/Advantages:

  • The anti-static ingredient is 100% concentrated in GYCAT-300B through the unique thermocompression technique
  • Provides outstanding anti-static performance
  • Effectively reduces the surface resistance value
  • Features great compatibility and processing behavior during the pellet compounding
  • Can be directly added or used for the applications of extrusion molding, injection molding, and blown film molding
  • With only little amount of adding rate
  • Ease of operating and produces no dust
  • Features great heat resistance
Applications:
  • Any plastics or elastomers
  • General plastic and engineering plastic
  • PA6, PA66, PA1010, PA610, etc.
  • EVA, PP, PE (HDPE, LDPE)
  • PET, PBT, etc.
  • Coatings, pigment, ink, powder paint
  • ABS, PS, EPS, PC, PMMA
  • Any polymers
  • Elastomers: TPS, PPR, TPO, TPV, TPEE, TPU PVC products
  • Silicone rubber, thermosetting resin
  • Packing materials, thin film, synthetic leather, sheet, electronic products
  • Any products that anti-static performance is highly required

Information provided by Go Yen Chemical

Vendors:
Available Properties
  • Ash
  • Acid Value
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.