MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Shell Carilon® DB6G6A10 Polyketone, 30% Glass-Reinforced General-Purpose Injection Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyketone; Polyketone, Glass Fiber Reinforced

Material Notes: Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6G6A10 is a 30 percent short glass-fiber-reinforced, general purpose injection molding grade, with mechanical properties that classify it as an engineering thermoplastic. This grade shows a unique balance of toughness and high modulus combined with good creep performance, strength and elevated temperature performance. Moreover this polymer exhibits a high resistance to hydrocarbons, solvents, salt solutions, weak acids and weak bases. CARILON Polymer DB6G6A10 is easy to process on standard injection molding equipment. Cycle times are generally short and parts show good mold definition. CARILON Polymers' low moisture sensitivity means that no conditioning of parts before assembly or use is necessary.

Data provided by Shell Chemical.

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570, 24 hour immersion
  • Moisture Absorption at Equilibrium, at 50% RH; ASTM D570
  • Water Absorption at Saturation, ASTM D570
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Linear Mold Shrinkage, Transverse, ASTM D955
  • Hardness, Shore D, ISO 868
  • Tensile Strength, Ultimate, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, at 5% strain; ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D256
  • Charpy Impact Unnotched, ISO 179
  • Charpy Impact, Notched, ISO 179
  • Charpy Impact, Notched, ISO 179
  • Electrical Resistivity, ASTM D257
  • Surface Resistance, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149, Short Term
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • Comparative Tracking Index, UL746A
  • Melting Point
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Flammability, UL94
  • Oxygen Index, ISO 4589
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.