MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Evonik Trogamid® BX9724 40% Glass Reinforced Nylon Blend  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6-3 (PA63)

Material Notes: Description: The TOGAMID® BX grades cover reinforced and non-reinforced blends based on PA 6-3-T and semi-crystalline polyamides. Non-reinforced blends are permanently transparent. Some blends have been developed in particular for manufacturing plastic-rubber composites. The special characteristics are:
  • high resistance to stress cracking
  • resistant to grease and fuels
  • good strength high hardness
  • very low mold shrinkage
  • very low tendency to warp
  • low moisture absorption
  • dimensionally stable even while absorbing water

The polyamide blends are especially suitable for the production of injection-molded parts subject to high thermal and mechanical stress. Thanks to their high stiffness moldings made from reinforced grades are appropriate for substituting cast metal parts, and are significantly lighter than these. Moldings exhibit outstanding surface qualities in spite of their high glass fiber content. TROGAMID® BX compounds can be combined with various rubber mixtures to produce plastic-rubber composite parts that are resistant to fuel and oil.

Specific Notes for this Material: Polymer blend consisting of amorphous and semi-crystalline polyamides, 40% glass fiber reinforced, with high tensile modulus for injection molding, dimensionally stable even while absorbing water; appropriate for substituting cast metal parts with plastic. Moldings exhibit outstanding surface qualities in spite of their high glass fiber content.

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Key Words: PA 6-3-T/XX, trimethyl hexamethylene diamine terephthalic acid
Vendors:
Available Properties
  • Density, ISO 1183
  • Viscosity Number, ISO 307
  • Hardness, Shore D, ISO 868
  • Ball Indentation Hardness, ISO 2039-1, H30
  • Tensile Strength at Break, ISO 527-1/2, 5 mm/min
  • Elongation at Break, ISO 527-1/2, 5 mm/min
  • Elongation at Break, ISO 178, 5 mm/min, Outer fiber strain
  • Tensile Modulus, ISO 527-1/2
  • Flexural Strength, ISO 178, 5 mm/min, at 3.5% Strain
  • Flexural Strength, ISO 178, 5 mm/min
  • Flexural Modulus, ISO 178
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA
  • Charpy Impact, Notched, ISO 179/1eA
  • Charpy Impact, Notched, ISO 179/1eA
  • Tensile Creep Modulus, 1 hour, ISO 899-1
  • Tensile Creep Modulus, 1000 hours, ISO 899-1
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • Surface Resistance, IEC 60093, Spec.
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243-1, K20/P50
  • Dissipation Factor, IEC 60250
  • Comparative Tracking Index, IEC 60112, Test Solution A, 100 drops
  • CTE, linear, ISO 11359, Longitudinal
  • CTE, linear, Transverse to Flow, ISO 11359
  • Melting Point, DSC, 10 K/min
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/2
  • Vicat Softening Point, ISO 306, 50N
  • Glass Transition Temp, Tg, Tg, 10 K/min
  • Flammability, UL94
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic
PA, Polyamide

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.