MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
3M Scotchkote™ MC 145 Epoxy Primer
Categories: Polymer; Thermoset; Epoxy

Material Notes: Scotchkote Epoxy Primer MC 145 is a solvent based two component primer suitable for use on a wide range of metallic and glass reinforced plastic (GRP) surfaces prior to the application of Scotchkote roofing system.

Product Features:

  • Combines good application characteristic with excellent adhesion to correctly prepared surfaces.
  • As a primer, it offers proven long term corrosion protection of ferrous and non ferrous metallic substrates.
  • Extended overcoating window for a wide range of top coats.
  • Can be applied by brush, roller or spray.

Information provided by 3M

Vendors:
Available Properties
  • Density
  • Solids Content
  • Volatile Organic Compounds (VOC) Content, as supplied
  • Volatile Organic Compounds (VOC) Content, thinned 10%
  • Thickness, Dry
  • Thickness, Wet
  • Cure Time, Touch Dry
  • Cure Time, Hard Dry
  • Cure Time, Full Cure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.