Notes: Telcar TL-2540A is a general purpose, low density thermoplastic elastomer designed for injection molding applications. Features:General Purpose; Good Colorability; High Flow; Low Density; Low Hardness; Low Specific Gravity; Oil Extended Uses: General Purpose; Grommets; Industrial Applications; Industrial Parts Form: Pellets Processing Method: Injection Molding; Extrusion Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpm Information Provided by Teknor Apex |