MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Lord Adhesives Chemglaze® V021 Polyurethane Coating  (discontinued **)
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where maximum performance properties are needed. These coatings provide the highest possible combinations of abrasion resistance, wear properties and flexibility. Use Chemglaze V-Line coatings as protective coatings for vinyl, Mylar®, ABS, FRP, and Noryl®.

Excellent wear is characteristic of all Chemglaze products. In laboratory evaluations 7.6 to 38.1 µm (0.3 to 1.5 mils) of Chemglaze V-Line polyurethane coatings provide better scuff and wear resistance than 50.8 - 76.2 µm (2 to 3 mils) of conventional scuff coats.

Extra Flexible Gloss

Socomore acquired the Aeroglaze® and Chemglaze® product lines from Lord in September 2016. This specific grade is discontinued and not a part of the Socomore product line.

Vendors:
Available Properties
  • Density, ASTM D1475
  • Solids Content, ASTM D2369 Modified, by volume
  • Solids Content, ASTM D2369 Modified, by weight
  • Volatile Organic Compounds (VOC) Content, ASTM D3960
  • Brookfield Viscosity, ASTM D2196, LVT, Spindle #2 @ 30rpm
  • Tensile Strength, Yield, Coatings catalyzed 2% with 9995, baked 15 minutes @ 107ºC, post cured 2 weeks @ 25ºC and 50% relative humidity. Free films tested on an Instron tester
  • Elongation at Yield, Coatings catalyzed 2% with 9995, baked 15 minutes @ 107ºC, post cured 2 weeks @ 25ºC and 50% relative humidity. Free films tested on an Instron tester
  • Flash Point, ASTM D3278, Seta Flash, Closed Cup
  • Cure Time
  • Cure Time
  • Cure Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.