MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Chemours Teflon® FEP 5100 Fluoropolymer Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Fluorinated Ethylene Propylene (FEP)

Material Notes: Teflon® FEP 5100 fluoropolymer resin is a meltprocessible fluoropolymer resin specifically designed for high-speed extrusion of thin coatings on small-gauge wires for twisted-pair constructions. As shown in Table 1, this resin provides the electrical and mechanical properties needed for low-voltage applications. In addition, Teflon® FEP 5100 has a higher melt flow rate than most other fluoropolymer resins. This permits higher extrusion speeds and easier processing, making Teflon® FEP 5100 a cost-effective alternative for producing thin-wall extrusions.

Teflon® FEP 5100 possesses a balance of processing and performance properties, which makes it an excellent choice for many applications. Like all Teflon® fluoropolymer resins, Teflon® FEP 5100 offers an excellent combination of properties:

  • chemical inertness
  • exceptional dielectric properties
  • heat resistance
  • toughness
  • flexibility
  • low coefficient of friction
  • nonstick characteristics
  • negligible moisture absorption
  • low flammability
  • performance at temperature extremes
  • weather resistance

Applications

Teflon® FEP 5100 is especially suitable for use in insulating data and telecommunications cables with excellent fire performance and physical properties as well as outstanding electrical performance. Cables insulated with Teflon® FEP 5100 can meet the requirements of Underwriters Laboratory “UL 910 Steiner Tunnel Test” for installation in plenums without metal conduits as is described in the National Electrical Code, Articles 725 and 800, and also complies with ASTM 2116-95a.

Teflon® FEP 5100 is not recommended as a jacket material or as an insulation in constructions where significant thermal cycling may be encountered.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Water Absorption, ASTM D570, 24 hours
  • Melt Flow, ASTM D2116
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, Ultimate, ASTM D1457
  • Elongation at Break, ASTM D1457
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Coefficient of Friction, ASTM D1894
  • Volume Resistivity, ASTM D257
  • Surface Resistivity per Square, ASTM D257
  • Dielectric Constant, ASTM D1531
  • Dielectric Strength, ASTM D149, 100 micrometers film
  • Dissipation Factor, ASTM D1531
  • Arc Resistance, ASTM D495
  • Melting Point, ASTM DTA E168
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  • Processing Temperature, Cure Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Chemours, former DuPont

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.