Amorphous Polycarbonate /Polyethylene Terephthalate Blend (PC/PET) Characteristics: High Strength, Rigidity and Creep Resistance. Good Chemical Resistance Applications: Pump Components, Industrial and Automotive Applications Processing: Injection Molding: Melt Temperature:500-540° F, Mold Temperature:170-240° F Data supplied by Albis Plastics Corporation. Former ALBIS Plastics product lines have been spun off under the MOCOM brand. This specific grade was discontinued prior to the spin off. |