MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Ho Hsiang Ching HR-550W SBS
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: The HR series belongs to the SBS(STYRENE- BUTADIENE-STYRENE BLOCK COPOLYMER) non-hydrogenated grade of materials. The HR series involving applications of footwear, mainly for abrasion resistance, softness, tear strength and other requirements. For example, a pair of comfortable shoes needs to be highly abrasion resistant, have a good grip along with other functions and provide a protective heel and a comfortable insole that breathes. This series is used in a wide range of shoes, including casual shoes, slippers and sport shoes. The HR series has adhesive properties and is thus able to work closely with other materials; it provides the functions for any shoes those basic requirements are wear-resistant and tough. Therefore, a good material made of elastic in scope of shoes, makes moving easier, that feels soft on the skin and comfortable for the legs to relieve fatigue Furthermore, it can be adapted for particular performances, for instance, with the excellent formula of thermoplastic elastomer material (TPE / TPS) and rubber resin blends, it favorably fulfills customers' special requirements for shoes! Our HR series is used fairly extensively in shoe materials, for both the appearance and functionality of shoe accessories, heels, soles and insoles are mostly being with satisfied Suitable for most of the thermoplastic processing methods, such as injection molding, extrusion molding and so on. This material complies with EU RoHS regulations, Polynuclear Aromatic Hydrocarbons (PAHs), REACH SVHC (Substances of Very High Concern), PFOS / PFOA and other safety tests.

Color: Transparent / Translucent/ Natural Color / Black Color / Customized Color

The optimum combination of materials: HIPS / PS

Processing: Injection, Extrusion

Storage conditions: At room temperature, avoid direct sunlight, keep away from fire and avoid humid environment.

Applications: Shoes, heels, insoles, toys, medical shoes, sporting goods, etc. Shoe Insole material is soft and fit well in the shoe foundation and can evenly distribute plantar pressure and relieve the discomfort of standing for long time. It can also protect the feet and increase the stability of traveling by foot. The Heel Counter position, as shown in the image, needs to be soft, supportive and cushioning. This can effectively increase the heel ability to withstand the pressure and friction. This part of the shoe is also known as the heel counter, it is used to stabilize the heel and to shape up the shoes.

Information provided by Ho Hsiang Ching Co., Ltd.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Melt Flow, ASTM D1238
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength, ASTM 412C
  • Elongation at Break, ASTM 412C
  • Tear Strength, ASTM 624C
  • Heat Distortion Temperature
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Mold Temperature
  • Injection Velocity
  • Injection Pressure
  • Hold Pressure
  • Back Pressure
  • Screw Speed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.