MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Chesterton ARC MXHT High temperature severe wear compound  (discontinued **)
Categories: Ceramic; Polymer; Thermoset; Epoxy

Material Notes: Description: An advanced ceramic composite for the protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack at elevated temperatures. It is applied at a thickness of 6mm (1/4”) or more. It is a 100% solids, non-shrinking coating. ARC MXHT is formulated with a high concentration of ceramic breads and fine ceramic particles for extremely abrasive environments where superior protection is needed. ARC MXHT is applied to a primed surface by trowel. It is chosen over ARC MX1 when abrasion resistance at elevated temperature is required.

Benefits:

  • Outlasts other wear resistant materials and coatings by 5-7 times
  • Excellent wear characteristics extend equipment’s operating cycles
  • Outperforms weld overlay or ceramic tiles
  • Tough resin structure resists thermal-mechanical shock.
  • Use in pH range 2-14 up to 130°C/266°F (wet service) and 230°C/466°F (dry service)
  • No need to post cure

Suggested Uses:Pumps

  • Elevated Temperature Fans/Blowers/Cyclones
  • Hoppers and Silos
  • Kiln Exhausters
  • Boiler Slag Systems
  • Electrostatic Precipitators

    Information provided by Chesterton

  • Vendors:
    Available Properties
    • Density, Cured
    • Hardness, Shore D, ASTM D2240
    • Tensile Strength at Break, ASTM D638
    • Elongation at Break, ASTM D638
    • Flexural Strength, ASTM D790
    • Flexural Modulus, ASTM D790
    • Compressive Strength, ASTM D695
    • Adhesive Bond Strength, ASTM D4541
    • Impact Test, ASTM D2794, Reverse
    • Maximum Service Temperature, Air, Wet Service
    • Maximum Service Temperature, Air, Dry Service
    • Cure Time, Light Load
    • Cure Time, Light Load
    • Cure Time, Light Load
    • Cure Time, Full Mechanical/Chemical
    • Cure Time, Full Mechanical/Chemical
    • Cure Time, Full Mechanical/Chemical
    • Tack-Free Time
    • Tack-Free Time
    • Tack-Free Time
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    none

    Category Notes
    Plastic

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Proto3000 – 3D Engineering Solutions
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.