MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
LyondellBasell Softell CA 7413 A Thermoplastic Olefinic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Softell CA 7413 A is a reactor TPO (thermoplastic polyolefin) manufactured using the LyondellBasell’s proprietary Catalloy process technology. It is suitable for the extrusion, calendaring and extrusion blow molding of very soft film and sheet as well as for injection molded parts. Softell CA 7413 A exhibits outstanding low stiffness, excellent low hardness and very good impact resistance. Softell CA 7413 A shows high compatibility to fillers and flame retardant additives as well as to other polyolefins. The grade is available in natural pellet form. Applications: Automotive Flooring, Interior Automotive Applications, Polymer Modifier, Single Ply Roofing, Soft Profile & Sheets, Soft Touch Applications, TPO Foils and Skins.

Information provided by LyondellBasell.

Vendors:
Available Properties
  • Density, ISO 1183-1, Method A
  • Melt Flow, ISO 1133-1
  • Hardness, Shore A, ISO 686
  • Tensile Strength at Break, ISO 527-1,-2
  • Elongation at Break, ISO 527-1,-2
  • Flexural Modulus, ISO 178
  • Charpy Impact, Notched, ISO 179
  • Charpy Impact, Notched, ISO 179
  • Charpy Impact, Notched, ISO 179
  • Melting Point, DSC, DSC
  • Vicat Softening Point, ISO 306, A50
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LyondellBasell (former Equistar)

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.