MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Master Bond EP113 Two Component Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced; Epoxy, High Temperature

Material Notes: Key Features:
  • Ultra low viscosity and very long open time
  • Cures with good toughness
  • Exceptionally low shrinkage upon curing
  • Superior dimensional stability
  • High temperature resistance
  • Stellar electrical insulation
Product Description: Master Bond EP113 is a two component, nano-silica filled epoxy system for potting, coating and sealing. The addition of the nano particles enhances the dimensional stability and the already exceptionally low shrinkage upon curing. EP113 has a 100 to 80 mix ratio by weight. It has an unusually low viscosity along with an especially long open time of 2-4 days. It should be noted that EP113 requires oven curing. A typical cure schedule is 2-3 hours at 250°F followed by 5-8 hours at 300°F with a 2 hour or longer post cure at 350°F, although, a number of variations are possible. EP113 is a top tier electrical insulator. It bonds well to a wide variety of substrates including metals, composites, glass, ceramics and plastics. As a toughened system, it has good resistance to thermal cycling and shock. When the aforementioned properties are combined with its pronounced low viscosity, it is a highly attractive candidate for potting and encapsulating. Some other positive features include its excellent physical strength profile as well as its chemical resistance to water, oils, acids, bases and fuels. The service temperature range is -100°F to +450°F. EP113 is a versatile, specialty type system that can be used in many different aerospace, electronic and OEM applications where this uncommon blend of product properties is desirable.

Product Advantages:

  • Low viscosity
  • Extraordinarily long open time
  • Can withstand rigorous thermal cycling
  • Marvelous electrical insulation properties
  • First rate physical properties
  • Great optical clarity

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, mixed
  • Viscosity, Part A
  • Hardness, Shore D
  • Tensile Strength
  • Tensile Modulus
  • Compressive Strength
  • Volume Resistivity
  • Volume Resistivity
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Constant
  • Dielectric Constant
  • Dielectric Constant
  • Dielectric Constant
  • Dielectric Constant
  • Dielectric Constant
  • Dissipation Factor
  • Dissipation Factor
  • Dissipation Factor
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, followed by 5-8 hours at 300°F with a 2 hour or longer post cure at 350°F
  • Working Life, After mixing, 100 g batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.