Product Description: PROAID AC 8XL is a highly concentrated, non-staining, non-discoloring processing and dispersing aid compatible with most polymers (including fluoroelastomers). HNBR flow and release properties are especially aided by AC 8XL. PROAID AC 8XL improves mold flow and extrusion characteristics as well as improving dispersion of fillers and chemicals. Mold and mill release are vastly improved with finished parts smooth and glossy. Mold buildup is greatly reduced and Proaid AC 8XL does not effect adhesion, bonding, or physical properties when used in recommended amounts. Will not interfere with peroxide cures.Information provided by Akrochem Corporation |