MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Teknor Apex TelcarĀ® TELC-87-L832-A Thermoplastic Elastomer
Categories: Polymer; Thermoplastic

Material Notes: Telcar TELC-87-L832-A is a general purpose thermoplastic elastomer designed for wire & cable applications requiring flexibility over a wide temperature range. It is a low density, medium hardness, low halogen content, UV stabilized grade that has good impact resistance and is suitable for extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Good Impact Resistance; Low Density; Low Halogen Content; UV Resistant

Uses: General Purpose; Wire & Cable Applications

RoHS Compliant:RoHS Compliant

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information provided by Teknor Apex

Vendors:
Available Properties
  • Density, ASTM D792
  • Viscosity, ASTM D3835
  • Melt Flow, ASTM D1238
  • Hardness, Shore A, ISO 868
  • Hardness, Shore A, ISO 888, Change in Air
  • Tensile Strength at Break, ASTM D412, Across Flow
  • Tensile Strength at Break, ASTM D412, Flow
  • Tensile Strength at Break, ISO 188, Across Flow, Change in Air
  • Tensile Strength at Break, ISO 188, Across Flow, Change in Air
  • Tensile Strength, ISO 188, Across Flow, Change in Air
  • Tensile Strength, ISO 188, Across Flow, Change in Air
  • Tensile Stress at Strain, ASTM D412, Across Flow
  • Tensile Stress at Strain, ASTM D412, Flow
  • Elongation at Break, ASTM D412, Flow
  • Elongation at Break, ASTM D412, Across Flow
  • Tear Strength, ASTM D624, Across Flow
  • Compression Set, ASTM D695
  • Compression Set, ASTM D695
  • Compression Set, ASTM D695
  • Dielectric Constant, ASTM D150
  • Brittleness Temperature, ASTM D746
  • Zone 1, Extrusion
  • Zone 2, Extrusion
  • Zone 3, Extrusion
  • Zone 5, Extrusion
  • Die Temperature, Extrusion
  • Screw Speed, Extrusion
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Teknor Apex Company

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.