MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Bostik Durabond® D-815™ Carpet Seam & Multi-Use Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: Description: DURABOND® D-815™ Carpet Seam & Multi-Use Adhesive is a fast grab, non-flammable adhesive for seaming and bonding carpet edges; tack strips; rubber cove base; rubber/metal reducers or stair treads. D-815 is suitable for use over dry surfaces including concrete and plywood.

Product Benefits:

  • Bonds carpet seams, reducers, tack strips, rubber cove base and stair treads
  • Unparalleled adhesive performance
  • Adheres to wood, ceramic, concrete and many other Surfaces
  • Reduces edge raveling
Performance Characteristics:
  • Fast grab
  • Non-flammable
  • Dries quickly
Suggested Uses: As a carpet seam adhesive, D-815 works well with many types of backings including: hot melt, unitary latex, woven, Axminster®, enhancer, Action Bac®, jute, rubber and outdoor carpet. As a tack strip adhesive, D-815 quickly adheres tack strip to concrete or plywood, and can be power stretched in as little as one hour. As a rubber and metal adhesive, D-815 acts as a fast-setting contact cement.

Information provided by Bostik

Vendors:
Available Properties
  • Density
  • Solids Content
  • Cure Time, Set Up Time
  • Cure Time, Final
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.