Approx. H+ equivalent weight 133. Mix Ratio with GY 6010 is 70. Comments/Applications: Modified polyamidoamine, low viscosity, solvent free. No induction, excellent gloss, chemical resistance. *Flexible mix ration - 70 to 100 phr, with GY 6010. High solids marine/maintenance primers, floorings, coatings. EPA potable water. Mil spec. 24441. Data provided by Ciba Specialty Chemicals. Ciba Specialty Chemicals has been acquired by Huntsman. |