MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Röhm ACRYLITE® Soundstop NT Acrylic based polymer  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Product: ACRYLITE® Soundstop NT CC is a highly filled, non-transparent grade of cast acrylic.

Properties: In addition to the well-known and proven properties of ACRYLITE®, such as

  • extremely high weather resistance
  • ease of fabrication
  • high surface hardness
  • low weight
  • 100% recyclability,
ACRYLITE® Soundstop NT offers the following special features:
  • Large noise barrier elements reduce the need for steel supporting structures.
  • ACRYLITE® Soundstop NT achieves the highest airborne sound reduction category (B3) of EN 1793-2, and also meets all requirements of EN 1794-1,2.
  • ACRYLITE® Soundstop NT is available in various colors.
  • ACRYLITE® Soundstop NT can be supplied with a matte or gloss surface.
  • Since the sheets are homogeneously colored, there is no flaking.
Applications: These properties make ACRYLITE® Soundstop NT especially suitable for
  • noise control along roads and railways
  • wind barriers on bridges

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors:
Available Properties
  • Density, ISO 1183
  • Tensile Strength at Break, ISO 527-2/1B/5
  • Elongation at Break, ISO 527-2/1B/5
  • Modulus of Elasticity, ISO 527-2/1B/5
  • Flexural Strength, ISO 178
  • CTE, linear, DIN 53752-A
  • Maximum Service Temperature, Air
  • Vicat Softening Point, ISO 306-B50
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Röhm GmbH , former product of Evonik Corporation; Evonik Cyro

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.