MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Aluminum 2024-T81
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: Information provided by Alcoa and the references. General 2024 characteristics and uses: Good machinability and surface finish capabilities. A high strength material of adequate workability. Has largely superseded 2017 for structural applications.

Uses: Aircraft fittings, gears and shafts, bolts, clock parts, computer parts, couplings, fuse parts, hydraulic valve bodies, missile parts, munitions, nuts, pistons, rectifier parts, worm gears, fastening devices, veterinary and orthopedic equipment, structures.

Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
A Zr + Ti limit of 0.20 percent maximum may be used with this alloy designation for extruded and forged products only, but only when the supplier and the purchaser have mutually agreed.
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 2024-T81; UNS A92024; ISO AlCu4Mg1; NF A-U4G1 (France); DIN AlCuMg2; AA2024-T81, ASME SB211; CSA CG42 (Canada); Al2024-T81
Vendors:
Available Properties
  • Density, AA; Typical
  • Hardness, Brinell, 500 kg load with 10 mm ball
  • Hardness, Knoop, Converted from Brinell Hardness Value
  • Hardness, Rockwell A, Converted from Brinell Hardness Value
  • Hardness, Rockwell B, Converted from Brinell Hardness Value
  • Hardness, Vickers, Converted from Brinell Hardness Value
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate, Flat sheet
  • Tensile Strength, Ultimate, Flat sheet
  • Tensile Strength, Ultimate, Wire, rod, bar and shapes (extruded)
  • Tensile Strength, Ultimate, Extruded tube
  • Tensile Strength, Ultimate, Wire, rod, bar and shapes (extruded)
  • Tensile Strength, Ultimate, Extruded tube
  • Tensile Strength, Yield
  • Tensile Strength, Yield, Flat sheet
  • Tensile Strength, Yield, Flat sheet
  • Tensile Strength, Yield, Wire, rod, bar and shapes (extruded)
  • Tensile Strength, Yield, Extruded tube
  • Tensile Strength, Yield, Wire, rod, bar and shapes (extruded)
  • Tensile Strength, Yield, Extruded tube
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Elongation at Break, Foil
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break, Flat sheet
  • Elongation at Break, Flat sheet
  • Elongation at Break, In 5 cm
  • Elongation at Break, Wire, rod, bar and shapes (extruded)
  • Elongation at Break, Extruded tube
  • Elongation at Break, Wire, rod, bar and shapes (extruded)
  • Elongation at Break, Extruded tube
  • Modulus of Elasticity, Average of Tension and Compression. In Al alloys, the compressive modulus is typically 2% greater than the tensile modulus
  • Poissons Ratio
  • Fatigue Strength
  • Shear Modulus
  • Shear Strength
  • Electrical Resistivity, AA; Typical
  • CTE, linear
  • CTE, linear
  • CTE, linear, AA; Typical; average over range
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity, AA; Typical at 77°F
  • Melting Point, AA; Typical range based on typical composition for wrought products >= 1/4 in. thickness. Eutectic melting is not eliminated by homogenization.
  • Solidus, AA; Typical
  • Liquidus, AA; Typical
  • Annealing Temperature
  • Solution Temperature
  • Aluminum, Al, As remainder
  • Chromium, Cr
  • Copper, Cu
  • Iron, Fe
  • Magnesium, Mg
  • Manganese, Mn
  • Other, each
  • Other, total
  • Silicon, Si
  • Titanium, Ti
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.