MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Saint-Gobain NortonĀ® V770 Low-Density Pressure Sensitive Adhesive Sealant Foam
Categories: Polymer; Adhesive; Thermoplastic; Vinyl (PVC)

Material Notes: Low Density Foam Suitable for Sealing of Thin Gauge Metals and Plastics. Closed cell polyvinyl chloride foam sealant with pressure sensitive adhesive on one side. The tight bonding adhesive keeps sealant in place during each stage of product assembly. The adhesive is on the non-linear side, making installation easier and quicker.

Features/Benefits:
  • 30% compression provides an excellent seal against light, dust and water in mechanically fastened assemblies
  • Excellent resistance to weather, fungi, and oxidation provides a long sealing life
  • Will not crack in cold temperatures
  • Superb closed cell structure of foam provides a positive seal
  • Low force to compress means faster and easier formation of a positive seal
  • Flexibility facilitates use in radius corners
  • Low density sealant allows easy assembly of large wall systems
Typical Applications: Curtainwall, precast concrete walls, refrigeration, telecommunications, pneumatic system seals, retail weatherstrip, bus and off-road vehicles, air conditioning, environmentally controlled rooms. All data based on a 0.25 inch test sample.(Available in thicknesses from 1/8" to 1/2".)
Information provided by Saint Gobain Performance Products.

Vendors:
Available Properties
  • Density, ASTM D1667
  • Water Absorption, NTP-35, % by volume
  • Hardness, Shore OO, ASTM D2240
  • Tensile Strength, Yield, ASTM D-412 (Die A)
  • Elongation at Break, ASTM D-412 (Die A)
  • Compressive Strength, ASTM D1667, Compression Deflection, Compressed to 30%.
  • Compressive Modulus, Force to Compress, Value for 30% compression.
  • Compression Set, Norton Test Procedure 37, Constant Deflection, Compressed to 30%.
  • Thermal Conductivity, ASTM-C-518
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saint Gobain Performance Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.