MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Angst+Pfister APSOplast® PF CC 201 Laminated fabric, Hgw 2082
Categories: Polymer; Thermoset

Material Notes: (laminated fabric sheets made from phenolic resin and fine cotton fabric)

Thanks to the use of fine cotton fabric, this laminated fabric has very good mechani cal properties. This construction grade is particularly suitable for parts with high demands in mechanical engineering. If value is placed upon particularly good dielectric properties – ensuring that parts are suitable for purposes where good insulation is required – type PF CC 202 (Hgw 2082.5) is recommended. This material is manufactured using special resins and electrolyte-free fabric.

Information provided by Angst + Pfister

Vendors:
Available Properties
  • Density, ISO 1183
  • Tensile Strength, ISO 527
  • Modulus of Elasticity, ISO 178, flexural test
  • Flexural Strength, ISO 178
  • Charpy Impact Unnotched, ISO 179/3C
  • Surface Resistance, IEC 60167, after 24 h immersed in water
  • Dielectric Constant, DIN 53483
  • Dielectric Strength, IEC 60243-1, at 90°C in oil parallel to layers
  • Comparative Tracking Index, IEC 60243-1, [kV], at 90°C in oil parallel to layers
  • CTE, linear, VDE 0304/2
  • Thermal Conductivity, DIN 52612
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.