MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Henkel Loctite® Stycast® ES 4512 Two-Component Epoxy Casting System
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Loctite Stycast ES 4512 provides the following product characteristics: Room temperature cure

Application: Potting and Encapsulating

Loctite Stycast ES 4512 is a two-component casting system with excellent handling properties. This low cost, flexible system is filled with a non-abrasive filler for machine metering/dispensing or regular hand mixer applications.

Information provided by Henkel.

Vendors:
Available Properties
  • Density, Part B
  • Density, Mixed
  • Density, Part A
  • Solids Content, Part A
  • Solids Content, Part B
  • Filler Content, Part A
  • Filler Content, Part B
  • Water Absorption, ISO 62
  • Viscosity, Mixed
  • Brookfield Viscosity, RVF, Spindle 5, speed 20 rpm, Part B
  • Brookfield Viscosity, Spindle 6, speed 20 rpm, Part A
  • Brookfield Viscosity, RVF, Spindle 6, speed 2 rpm, Part A
  • Linear Mold Shrinkage, ASTM D792
  • Hardness, Shore D, ISO 868
  • Tensile Strength, ISO 527-2, Hysol
  • Elongation at Break, ISO 527-2
  • Flexural Strength, ISO 178
  • Compressive Strength, ISO 604, Hysol
  • Tear Strength, ISO 34-2, Die D, Hysol
  • Volume Resistivity, IEC 60093
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • Surface Resistance, IEC 60093
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243-1
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • CTE, linear, ASTM D7012, Pre Tg (Alpha 1)
  • CTE, linear, ASTM D7012, Post Tg (Alpha 2)
  • Thermal Conductivity, ISO 8302
  • Glass Transition Temp, Tg, ISO 11357-2
  • Flammability, UL94
  • Cure Time, Alternate
  • Cure Time, Recommended
  • Pot Life, 200 g mass
  • Gel Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Loctite Division of Henkel

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.