MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Syensqo (Solvay Specialty Polymers) Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes: AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, plus superior thermal performance to resist blistering during lead-free SMT processes.

Color stability is enhanced compared to previous flame-retarded grades. Quick crystallization in water-cooled molds allows for fast cycle times using mold temperatures as low as 150°F (65°C).

Information provided by Solvay Advanced Polymers

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Specific Gravity, ISO 1183A
  • Moisture Absorption at Equilibrium, ASTM D570, 24 hours
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength, Yield, ISO 527
  • Tensile Strength, Yield, ASTM D638
  • Tensile Strength, Yield, ISO 527
  • Tensile Strength, Yield, ISO 527
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Elongation at Break, ISO 527
  • Elongation at Break, ISO 527
  • Elongation at Break, ISO 527
  • Elongation at Yield, ASTM D638
  • Tensile Modulus, ISO 527
  • Tensile Modulus, ASTM D638
  • Tensile Modulus, ISO 527
  • Tensile Modulus, ISO 527
  • Tensile Modulus, ISO 527
  • Flexural Strength, ISO 178
  • Flexural Strength, ASTM D790
  • Flexural Strength, ISO 178
  • Flexural Strength, ISO 178
  • Flexural Strength, ISO 178
  • Flexural Modulus, ISO 178
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ISO 178
  • Flexural Modulus, ISO 178
  • Flexural Modulus, ISO 178
  • Compressive Strength, ASTM D695
  • Shear Strength, ASTM D732
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D4812
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Izod Impact, Unnotched (ISO), ISO 180/1U
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA
  • Volume Resistivity, ASTM D257
  • Surface Resistance, ASTM D257
  • Dielectric Strength, ASTM D149
  • Dielectric Strength, ASTM D149
  • Comparative Tracking Index
  • Hot Wire Ignition, HWI, UL 746A
  • High Amp Arc Ignition, HAI, UL 746A
  • Melting Point, ASTM D3418
  • Melting Point, ISO 11357-3
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75Af
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.