MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Solvay MTM® 29SFR Epoxy Resin
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: MTM29SFR pregrepgs are controlled flow, 120°C (248°F) curing, halogen-free, flame-retarded epoxy materials offering flexible processing and handling characteristics. MTM29SFR has been developed specifically for rail applications and can be processed by oven vacuum bag, press molding and autoclave. These prepregs exhibit a good balance of mechanical properties and, after a suitable cure, can be used at temperatures up to 80°C (176°).

Features & Benefits:

  • 30 days out life at 21°C (70°F)
  • 12 months storage life at -18°C (0°F)
  • Versatile processing: oven vacuum bag, autoclave and press molding
  • Can be cured 80 to 135°C (176 to 275°F)
  • Service temperature up to 80° (176°F)
  • Meets the fire requirements of DIN 5510, classes S4, SR2 and ST2, with a toxicity: 30 minutes FED=0.176
  • Meets the fire requirements of BS6853 Category 1b (exteriors and Category II (interiors)
Note 1: Material: MTM24SFR/600 g/m2 2x2 twill E-glass fiber;

Information provided by Cytec, subsequently acquired by Solvay.

Vendors:
Available Properties
  • Density, Cured Resin
  • Storage Temperature
  • Tensile Strength, ISO 527-4, 0°, Note 1, Press: 1 hrs at 125°C
  • Tensile Strength, ISO 527-4, 0°, Note 1, Oven vacuum bag: 8 hrs at 85°C
  • Tensile Modulus, ISO 527-4, 0°, Note 1, Press: 1 hrs at 125°C
  • Tensile Modulus, ISO 527-4, 0°, Note 1, Oven vacuum bag: 8 hrs at 85°C
  • Flexural Strength, ISO 178, 0°, Note 1, Oven vacuum bag: 8 hrs at 85°C
  • Flexural Strength, ISO 178, 0°, Note 1, Press: 1 hrs at 125°C
  • Flexural Modulus, ISO 178, 0°, Note 1, Oven vacuum bag: 8 hrs at 85°C
  • Flexural Modulus, ISO 178, 0°, Note 1, Press: 1 hrs at 125°C
  • Compressive Strength, EN2850, 0°, Note 1, Press: 1 hrs at 125°C
  • Compressive Strength, EN2850, 0°, Note 1, Oven vacuum bag: 8 hrs at 85°C
  • Shear Strength, ASTM D2344, 0° Interlaminar, Note 1, Oven vacuum bag: 8 hrs at 85°C
  • Shear Strength, ASTM D2344, 0° Interlaminar, Note 1, Press: 1 hrs at 125°C
  • Maximum Service Temperature, Air
  • Glass Transition Temp, Tg, DMA E' onset Tg, 1 hr at 120°C, wet
  • Glass Transition Temp, Tg, DMA E' onset Tg, 1 hr at 120°C, dry
  • Cure Time, 125°C
  • Cure Time, 80
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.