MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Avient Polystrand ThermoBallistic™ TBE8010X X-Ply Cross-Ply Polypropylene-Glass Composite  (discontinued **)
Categories: Polymer; Tape; Thermoplastic; Polypropylene (PP)

Material Notes: 2-Ply with Fiber Orientation at 0° & 90°.

. Polystrand ThermoBallistic laminates combine continuous E-Glass (ThermoBallistic-E™) structural fibers with a proprietary polypropylene thermoplastic polymers to form sheets, ribbons or tapes that can be subsequently molded to create end-use applications including ballistic and blast panels to protect troops, vehicles, equipment and buildings.

The Polystrand materials and process technologies combine continuous structural fibers with an energy-dissipating matrix of thermoplastic polymer. This results in a reinforced thermoplastic composite that has many advantages compared to traditional, more brittle thermosetting polymer composites in ballistic panels. The many performance benefits of Polystrand ThermoBallistic materials include:

  • Exceptional Energy Management Properties (ballistic, blast and high strain-to-failure)
  • Improved V50 Performance Against a 30 Caliber FSP (ThermoBallistic E)
  • Lighter Weight (automotive, aircraft and defense applications)
  • X-Ply™ 0/90 Laminates up to 50" x 100" (1.27m x 2.54m) and rolls
  • 100% Recyclable (no material waste)
  • Reduced Molding Cycles (higher productivity and lower cost)
  • Re-Formable (panels can be reconfigured multiple times)
  • Design Flexibility (fiber selection and fiber orientation)

Information provided by Polystrand.

Vendors:
Available Properties
  • Density
  • Filler Content, ASTM D2584, E-Glass
  • Thickness
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Polystrand, Inc.

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.