MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
GEHR Plastics PET Polyethylene Terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Polyethylene terephthalate shows high tensile and mechanical strength, hardness and toughness, low friction and a high dimensional stability. PET may be used at temperatures ranging from -20°C to approximately 115°C.

Properties

  • high mechanical resistance and tensile strength
  • high surface strength
  • easy to varnish and polish
  • high dimensional stability
  • high toughness
  • good electrical insulating properties
  • high chemical resistance
  • limited dielectric properties
  • sensitive to hydrolysis
Applications include bearings, pumps and parts for housings, frame components, tank lids, cogwheels, insulators for the electrotechnic, deflection rollers for the filament industry, levers, handles, and control disks.

Vendors:
Available Properties
  • Specific Gravity, ISO 1183
  • Moisture Absorption at Equilibrium, ISO 62
  • Water Absorption at Saturation, ISO 62
  • Hardness, Rockwell M, ISO 2039
  • Hardness, Shore D, ISO 868
  • Ball Indentation Hardness, ISO 2039
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Elongation at Yield, ISO 527
  • Modulus of Elasticity, ISO 527
  • Charpy Impact Unnotched, ISO 179
  • Charpy Impact Unnotched, ISO 179, round rods 220-300mm
  • Charpy Impact Unnotched, ISO 179, round rods 160-200mm
  • Charpy Impact, Notched, ISO 179
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243-1
  • Dielectric Loss Index, IEC 60250
  • Comparative Tracking Index, IEC 60112
  • CTE, linear, ISO 11359
  • Thermal Conductivity, ISO 22007-4
  • Melting Point, DIN EN ISO 3146
  • Maximum Service Temperature, Air, UL 746B
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75
  • Minimum Service Temperature, Air, UL 746B
  • Glass Transition Temp, Tg, DIN EN ISO 3146
  • Flammability, UL94, UL 94
  • Oxygen Index, ASTM D2863
  • FDA, Physiological indifference
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
GEHR Plastics Inc

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.