MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Trinseo MAGNUM™ 8434 ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Product Description: MAGNUM™ 8434 is a medium heat ABS. It is suitable for interior automotive applications requiring high gloss.
Benefits: Lot to lot consistency for optimal machine parameters setting from the start; Low VOC allowing a better interior air quality facing increasing regulatory and OEMs constraints; Heat stability during wide range of processing temperatures: enhanced part design freedom
Applications: Various covered interior trims; Painted Grilles and Other Exterior Trims

Complies with: US FDA 21 CFR 181.32

Availability: Europe; Latin America; North America

Features: Good Processability; High Gloss; High Heat Resistance: Paintable

Uses: Appliances; Automotive Applications; Automotive Interior Parts; Toys

Automotive Specifications: FORD WSS-M4D827-A3 Color: Natural: GM QK 002022 Color: Natural

Form: Pellets

Processing Method: Injection Molding

Information provided by Trinseo

Vendors:
Available Properties
  • Bulk Density, ISO 60
  • Density, ISO 1183
  • Linear Mold Shrinkage, ISO 294-4
  • Melt Flow, ISO 1133
  • Tensile Strength, Yield, ISO 527-2/50
  • Elongation at Break, ISO 527-2/50
  • Elongation at Yield, ISO 527-2/50
  • Tensile Modulus, IOS 527-1/1
  • Flexural Strength, ISO 178, 0.079 in/min
  • Flexural Modulus, ISO 178, 0.079 in/min
  • Charpy Impact, Notched, ISO 179/1eA, Injection Molded
  • Vicat Softening Point, ISO 306/B50
  • Flammability, UL94
  • Flammability, UL94
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Trinseo, former Styron

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.