MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Phillips 66 Coupling Grease NLGI Grade 0.5
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Coupling Grease is a high-performance, polymer-containing lithium grease developed for use in grease-lubricated flexible couplings, such as those commonly found in mining equipment, power plants, manufacturing plants and chemical plants. It has exceptional resistance to oil separation when subjected to the high centrifugal forces typically encountered with medium- and high-speed gear, metallic grid and chain couplings. Coupling Grease is specifically formulated to the lower (softer) end of the NLGI No. 1 grade to meet most OEM requirements. It is manufactured with high-quality, high-viscosity base oils and lithium 12-hydroxystearate soap thickener. It is fortified with special extreme-pressure (EP) additives, oxidation and corrosion inhibitors and polymers to withstand the centrifugal action in couplings and adhere to the moving parts to provide lubrication, minimize friction and help extend coupling life. It has outstanding performance in the Koppers K36 Centrifugal Oil Separation Test.

Applications:

  • Gear, metallic grid and flexible-chain couplings
  • Couplings commonly used in mining and gas field equipment
  • Couplings and universal joints operating under high centrifugal forces
  • Couplings used between electric motors and gearboxes in industrial and chemical plants
Coupling Grease meets the requirements of the following industry specifications:
  • ANSI/AGMA Standard 9001-B97, Type CG-1 and CG-2 for medium- and high-speed couplings
Features/Benefit:
  • Outstanding resistance to oil separation
  • Excellent oxidation resistance and thermal stability
  • Protects against rust and corrosion
  • High load-carry ability
  • Minimizes friction and wear to help extended coupling life

Information provided by Phillips 66 Lubricants.

Vendors:
Available Properties
  • Density
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Oxidative Stability, ASTM D942, Pressure Drop
  • Four Ball Extreme Pressure, Weld Load, ASTM D2596
  • Four Ball Wear, ASTM D2266, Scar Diameter
  • Penetration, ASTM D217, Worked (10,000 strokes)
  • Penetration P(60), 1/10 mm, ASTM D217
  • Timken Test, ASTM D2509, OK Load
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Dropping Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.