MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Stratasys® Antero™ 800NA PEKK-based FDM 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyketone; PEKK, Unreinforced

Material Notes: Antero™ 800NA is a PEKK-based FDM® thermoplastic with excellent mechanical properties that include high strength, high heat resistance, toughness and wear-resistance. These qualities make it a lighter alternative to aluminum and steel in certain use cases. Chemical resistance and minimal outgassing provide suitability for aerospace applications where prototypes and parts are exposed to jet fuel, oil and hydraulic fluid. Other uses include industrial applications where high-strength and chemical resistance are needed. 3D printing with Antero 800NA FDM filament avoids the waste associated with subtractive manufacturing of high-cost bulk PEKK material.

Information provided by Stratasys.

Vendors:
Available Properties
  • Specific Gravity, ASTM D257, XY, XZ/ZX Orientations
  • Tensile Strength at Break, ASTM D638, ZX Orientation, Fortus 450mc w/T20D tip
  • Tensile Strength at Break, ASTM D638, ZX Orientation, F900 w/T20D tip
  • Tensile Strength at Break, ASTM D638, XZ Orientation, F900 w/T20D tip
  • Tensile Strength at Break, ASTM D638, XZ Orientation, Fortus 450mc w/T20D tip
  • Tensile Strength, Yield, ASTM D638, XZ Orientation, F900 w/T20D tip
  • Tensile Strength, Yield, ASTM D638, XZ Orientation, Fortus 450mc w/T20D tip
  • Elongation at Break, ASTM D638, ZX Orientation, Fortus 450mc w/T20D tip
  • Elongation at Break, ASTM D638, ZX Orientation, F900 w/T20D tip
  • Elongation at Break, ASTM D638, XZ Orientation, F900 w/T20D tip
  • Elongation at Break, ASTM D638, XZ Orientation, Fortus 450mc w/T20D tip
  • Elongation at Yield, ASTM D638, XZ Orientation, F900 w/T20D tip
  • Elongation at Yield, ASTM D638, XZ Orientation, Fortus 450mc w/T20D tip
  • Modulus of Elasticity, ASTM D638, XZ Orientation, F900 w/T20D tip
  • Modulus of Elasticity, ASTM D638, ZX Orientation, F900 w/T20D tip
  • Modulus of Elasticity, ASTM D638, XZ Orientation, Fortus 450mc w/T20D tip
  • Modulus of Elasticity, ASTM D638, ZX Orientation, Fortus 450mc w/T20D tip
  • Flexural Strength, ASTM D790, Procedure A, ZX Orientation, Fortus 450mc w/T20D tip
  • Flexural Strength, ASTM D790, Procedure A, XZ Orientation, F900 w/T20D tip
  • Flexural Strength, ASTM D790, Procedure A, XZ Orientation, Fortus 450mc w/T20D tip
  • Flexural Strength, ASTM D790, Procedure A, ZX Orientation, F900 w/T20D tip
  • Flexural Modulus, ASTM D790, Procedure A, ZX Orientation, F900 w/T20D tip
  • Flexural Modulus, ASTM D790, Procedure A, ZX Orientation, Fortus 450mc w/T20D tip
  • Flexural Modulus, ASTM D790, Procedure A, XZ Orientation, F900 w/T20D tip
  • Flexural Modulus, ASTM D790, Procedure A, XZ Orientation, Fortus 450mc w/T20D tip
  • Flexural Strain at Break, ASTM D790, Procedure A, ZX Orientation, Fortus 450mc w/T20D tip
  • Flexural Strain at Break, ASTM D790, Procedure A, ZX Orientation, F900 w/T20D tip
  • Compressive Yield Strength, ASTM D695, ZX Orientation, F900 w/T20D tip
  • Compressive Yield Strength, ASTM D695, XZ Orientation, F900 w/T20D tip
  • Compressive Yield Strength, ASTM D695, XZ Orientation, Fortus 450mc w/T20D tip
  • Compressive Yield Strength, ASTM D695, ZX Orientation, Fortus 450mc w/T20D tip
  • Compressive Modulus, ASTM D695, ZX Orientation, F900 w/T20D tip
  • Compressive Modulus, ASTM D695, ZX Orientation, Fortus 450mc w/T20D tip
  • Compressive Modulus, ASTM D695, XZ Orientation, F900 w/T20D tip
  • Compressive Modulus, ASTM D695, XZ Orientation, Fortus 450mc w/T20D tip
  • Izod Impact, Notched, ASTM D256, ASTM D4812, ZX Orientation, F900 w/T20D tip
  • Izod Impact, Notched, ASTM D256, ASTM D4812, ZX Orientation, Fortus 450mc w/T20D tip
  • Izod Impact, Notched, ASTM D256, ASTM D4812, XZ Orientation, Fortus 450mc w/T20D tip
  • Izod Impact, Notched, ASTM D256, ASTM D4812, XZ Orientation, F900 w/T20D tip
  • Izod Impact, Unnotched, ASTM D256, ASTM D4812, ZX Orientation, Fortus 450mc w/T20D tip
  • Izod Impact, Unnotched, ASTM D256, ASTM D4812, ZX Orientation, F900 w/T20D tip
  • Izod Impact, Unnotched, ASTM D256, ASTM D4812, XZ Orientation, F900 w/T20D tip
  • Izod Impact, Unnotched, ASTM D256, ASTM D4812, XZ Orientation, Fortus 450mc w/T20D tip
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150, XY, XZ/ZX Orientations
  • Dissipation Factor, ASTM D150, XY, XZ/ZX Orientations
  • CTE, linear, ASTM E831, XY Orientation
  • CTE, linear, ASTM E831, XZ/ZX Orientation
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648 Method B, XY, XZ/ZX Orientations
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648 Method B, XY, XZ/ZX Orientations
  • Glass Transition Temp, Tg, ASTM D7426, Inflection Point, XY, XZ/ZX
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.