MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Chemours Krytox™ GPL-407 PFPE Grease
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: Krytox™ GPL-407 grease is made using a non-melting thickener, instead of the normal Krytox™ PTFE. This change from PTFE to silica boosts the temperature capability of the grease to an upper limit determined by the evaporation/breakdown temperature of the oil. Krytox™ GPL-407 is made from Krytox™ GPL-107 oil, which, with proper ventilation, can withstand up to 399 °C (750 °F) and higher temperatures for brief periods. With replenishment/re-lubrication, it can last longer. While Krytox™ GPL-407 is not meant to replace the Krytox™ GPL-200 series at temperatures below 288–316 °C (550–600 °F), it does extend the range for using fluorinated greases to beyond the 316 °C (600 °F) limit of PTFE and Teflon™ thickened greases. Krytox™ GPL 407 has higher oil separation than PTFE thickened greases and, therefore, might not last as long under equivalent conditions.

Information provided by Chemours Krytox

Vendors:
Available Properties
  • Viscosity Measure, base oil
  • Viscosity Measure, base oil
  • Viscosity Measure, base oil
  • Viscosity Measure, base oil
  • Viscosity Measure, base oil
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Chemours, former DuPont Performance Lubricants

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.