  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
3M Nextel™ 440 Industrial Ceramic Fiber
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide; Other Engineering Material; Composite Fibers

Material Notes: Chemical composition above is wt%. Crystal phases are gamma alumina + mullite + amorphous SiO2. Filament diameter is 10-12 µm.

3M Nextel fibers 312, 440, and 550 are designed for non-structural applications where their primary purpose is to act as a flame barrier. 3M Nextel Ceramic Fiber 440 is made from Al2O3, SiO2, and B2O3. Because B2O3 is present, this composition has both crystalline and glassy phases. The glassy phase helps the fiber retain strength after exposure to high temperatures because it slows the growth of crystalline phases that weaken the fiber. However, when the fiber is stressed at high temperature, the glassy phase weakens the fiber due to viscous flow much like a glass fiber.

Information provided by 3M Ceramic Textile and Composites.

Key Words: Alumina, Aluminum Oxide
Vendors:
Available Properties
  • Density
  • Particle Size, Crystal size
  • Specific Surface Area
  • Tensile Strength, Ultimate, filament
  • Tensile Modulus, Filament property
  • Dielectric Constant
  • Dissipation Factor
  • CTE, linear
  • Specific Heat Capacity
  • Melting Point
  • Refractive Index
  • Al2O3
  • B2O3
  • SiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.