Features: Characteristics: Good impact & tear strength, High speed & superior heat sealing properties Additives: Anti-oxidants, LubricantsApplication: Shopping bags, Thin films, Trash bags, Multiwall bag liners, Polygloves CAS No. 25213-02-9 Information provided by LG Chemical |