MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Crucible Steel Nu-Die® XL (Premium Quality AISI H13) Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel; Air-Hardening Steel

Material Notes: Nu-Die XL (AISI H13) is a premium version of H13 tool steel manufactured, tested and certified to meet stringent die casting industry specifications issued by NADCA, Chrysler and others. It offers better transverse toughness than standard H13, reducing the susceptibility to breaking or cracking. Nu-Die XL is double melted and specially processed to improve its microstructural uniformity and microcleanliness, making it an excellent choice for critical polishability and more resistant to thermal fatigue. Nu-Die XL can be used in any application where standard H13* is used. Crucible stocks Nu-Die XL primarily in blocks and flats in the annealed condition.

H13 is a versatile, air-hardenable hot work tool steel providing moderate wear resistance along with good toughness, good heat check resistance, and high temperature strength up to 1000°F (540°C) with brief exposures up to 1100°F (595°C).

Information provided by Crucible Specialty Metals.

Vendors:
Available Properties
  • Density
  • Hardness, Brinell, Annealed
  • Hardness, Rockwell C, Austenitizing Temperature- 1010°C, air cool, Tempering Temperature- 605°C
  • Hardness, Rockwell C, Austenitizing Temperature- 1010°C, air cool, Tempering Temperature- 540°C
  • Modulus of Elasticity
  • Charpy Impact, Austenitizing Temperature- 1010°C, air cool, Tempering Temperature- 540°C
  • Charpy Impact, Austenitizing Temperature- 1010°C, air cool, Tempering Temperature- 605°C
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Thermal Conductivity
  • Thermal Conductivity
  • Shrinkage, Tempered at 400°F
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As Remainder
  • Molybdenum, Mo
  • Silicon, Si
  • Sulfur, S
  • Vanadium, V
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.